Earl Brunner on thu 6 jul 00


I do. What model is it. If it is the very small one that
is the one i have (small being relative in this case) Mine
is the model 802. I would be happy to discuss off list.
Geil would probably be happy to send you an owners manual if
you don't have one.

claypots wrote:
>
> Hello: Does anyone on the list have a Geil fiber lined gas
> downdraft kiln? I purchased a used one and am just now getting
> it hooked up. Since I don't have too much experience firing
> reduction, I would love to hear about firing schedules used for
> cone 10 reduction in this style kiln. Any info. would be
> appreciated. You can e-mail me at
> mailto:claypots@lynchburg.net. Thanks in advance.
> Debra
>
> ______________________________________________________________________________
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at melpots@pclink.com.

--
Earl Brunner
http://coyote.accessnv.com/bruec
mailto:bruec@anv.net

claypots on thu 6 jul 00


Hello: Does anyone on the list have a Geil fiber lined gas
downdraft kiln? I purchased a used one and am just now getting
it hooked up. Since I don't have too much experience firing
reduction, I would love to hear about firing schedules used for
cone 10 reduction in this style kiln. Any info. would be
appreciated. You can e-mail me at
mailto:claypots@lynchburg.net. Thanks in advance.
Debra