Sarah House on mon 10 jul 00
Oh well, maybe i'll try it anyway, It did come to mind a little later that
copper would work a lot better than iron for raku. thanks anyway
Sarah
Pat/Kent on tue 11 jul 00
You can try, Sarah, But Madame Dufuss here was so excited with black copper
oxide that she missed by a country mile. It is a good effect if you are
looking for coppers, but doesn't do much to replace I ron oxide.
I guess I'll just slink back into my cage, Maybe Kent will let me out next
week if i'm real good
Pat Porter
----- Original Message -----
From: "Sarah House"
To:
Sent: Friday, July 07, 2000 11:30 PM
Subject: black iron ox
> That sounds great! i'll try it next week, thanks for the reply.
> Sarah House
>
>
| |
|