search  current discussion  categories  kilns & firing - raku 

transp. raku receipe..........wrong

updated wed 12 jul 00

 

Alisa and Claus Clausen on tue 11 jul 00


Dear Clayart,
It seems jetlagged and completely kaput, I turned to my brain for info. =
too early.
80/20 Cornwall stone/Neph. sye is not correct.
It was of course 80/20 GB/Cornwall stone, which is no help.

I am thinking, since GB,Cornwall stone and Neph. Sye are all grouped as =
feldspathic fluxes, (different comps. of course)
I will try my fantasie receipe anyway.

More remotely intellegent comments when I come too myself again.
Sorry,=20
Best regards,
Alisa in Denmark