mel jacobson on wed 12 jul 00


sorry if i got taken in on the buildings thing...have never seen that
one before...but, hey let's not get rude about it. use the delete key.


spooze
1 cup sugar...any kind, honey, sugar, sugar syrup
1 cup vinegar, any kind
1 cup slip of your choice, you choice of thickness.

karo is corn syrup...and i misspelled it.
the reason i suggest corn syrup is that every house in america
has a jar that is about 40 years old...good use for it. i just ran and
checked our basement supplies and found a jar that had to have been
purchased in 1966.

mel


FROM MINNETONKA, MINNESOTA, USA
http://www.pclink.com/melpots (website)

Deeclay@AOL.COM on wed 12 jul 00


Good morning everyone.
I know about vinegar and slip but can you explain the use of sugar?
Thanks for all the good advise, recipies and interesting insites to potters
minds.
Diane in Miami trying my hand at yo-yo boxes in porcelain

Pottery by Dai on wed 12 jul 00


Hi, Diane in Miami - what is a yo-yo box??
Dai in Kelowna (where the .htm was outside the "box", Ken---and obviously my
brain isn't. I'm red-faced!)
potterybydai@home.com
There is an alarming increase in the number of things that I know nothing
about.
-----Original Message-----
From: Deeclay@AOL.COM
To: CLAYART@LSV.CERAMICS.ORG
Date: Wednesday, July 12, 2000 6:46 AM
Subject: Re: spooze,karo,spam


>Good morning everyone.
>I know about vinegar and slip but can you explain the use of sugar?
>Thanks for all the good advise, recipies and interesting insites to potters
>minds.
> Diane in Miami trying my hand at yo-yo boxes in porcelain
>
>___________________________________________________________________________
___
>Send postings to clayart@lsv.ceramics.org
>
>You may look at the archives for the list or change your subscription
>settings from http://www.ceramics.org/clayart/
>
>Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.

Tommy Humphries on wed 12 jul 00


karo syrup also makes an excellent binder/hardener for glazes, ala cmc.
smells like a candy factory during glaze firing!

Tommy


----- Original Message -----
From: "mel jacobson"
To:
Sent: Wednesday, July 12, 2000 7:04 AM
Subject: spooze,karo,spam


> sorry if i got taken in on the buildings thing...have never seen that
> one before...but, hey let's not get rude about it. use the delete key.
>
>
> spooze
> 1 cup sugar...any kind, honey, sugar, sugar syrup
> 1 cup vinegar, any kind
> 1 cup slip of your choice, you choice of thickness.
>
> karo is corn syrup...and i misspelled it.
> the reason i suggest corn syrup is that every house in america
> has a jar that is about 40 years old...good use for it. i just ran and
> checked our basement supplies and found a jar that had to have been
> purchased in 1966.
>
> mel
>
>
> FROM MINNETONKA, MINNESOTA, USA
> http://www.pclink.com/melpots (website)
>
>
____________________________________________________________________________
__
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.
>

Loraxwoods@AOL.COM on wed 12 jul 00


I now have the recipe but don't know what you use SPOOZE for, please explain.

Thanks, Nora