Hi, My husband built me the tile press. Unfortunately, I don't find it very
useful for large tiles. I think it even says that in the book. It's great
for the 4" tiles or smaller when I'm in big production mode. I also found
that some of my tiles that I pressed that were 5" or bigger developed cracks.
Every now and then I dust it off to use. I'll be doing that soon for my
niece's 3" wedding tile, 200 to be given as gifts to the guests at the
reception.

I don't know if that answers you're question, if not just say.

Good Luck,

Nancy G.