Dear Alisa,
The clear glaze from those recipes works well in oxidation with .25%
copper carb. it is a very nice matt celedon color. The glaze fits the
Archie Bray ^6 porcelain perfectly, no crazing.
If it crazes on your porcelain, then it is the fit. Adjustments would
need to be made.
The "Sexy Black" in ^6 0xidation is a rather nice brown- pumpkin or
oakleaf in color.
Best wishes,
Marcia
--