Sheron Roberts on fri 21 jul 00


The lowest I have
fired Phoenix to has
been cone 8. I must
say, my cone 10=20
glazes all are more
appealing when fired
to that temperature.
I have also fired=20
Highwater's Half=20
and Half, a white
stoneware/porcelain
body to cone 8 with
good results.