wedging table: after the plaster.

updated wed 26 jul 00

 

Kim Marie on tue 25 jul 00


I do use a plaster wedging table but have eliminated the plaster scare by
stapling painting canvas to the wood frame of the box I poured the plaster
into. Works for me!
Kim
Rural NY