Caroline Montague on thu 27 jul 00
Candace,
Trina Buff, Aurora, Craggie Crunch, Orange Stone and Phoenix, all of =
these clays from Highwater we have thrown, handbuilt, glazed and fired =
to ^10R. Phoenix, a light grey stoneware has been our choice for 3 years =
with no cracking problems in plates, bowls, altered shapes or =
attachments. It is a clean clay that does not stick to your fingers, has =
a nice presence and will just sit up on the batt and dry off looking =
great after you have thrown it or stretched it into a new =
shape.Beautiful clay.
Caroline Montague
montague@rabun.net
| |
|