Alisa and Claus Clausen on sat 29 jul 00


Dear Grace,
Although it has G. B. which may a problem to aquire,
it is a functional, high gloss clear that is simple

48 Gerstley Borate
30 Silica
22 K=E1olin =20

I have used over my engobes with sucess, but of course test your own.

Ron Roy's satin matt is a very smooth nice clear, less glossy and no =
G.B.

30 G-200
20 Walloastonite
30 EPK
30 3134

Good luck