gas firing

updated mon 31 jul 00

 

JODO96@AOL.COM on sun 30 jul 00


Well, I finally got the nerve to fire our kiln on my own. With an occasional
consult with my husband. Made it to cone 10 without any trouble felt the
reduction went well, kept accurate records, checked temp every 30 minutes and
logged every thing I could think of, we are going to put into the computer
and graft the firing. By doing this I know feel more confident about this
aspect of the process and will do it again next month. I learned a lot and of
course have much more to go. What Fun!

Dorothy
Manakin-Sabot, Va.