Edouard Bastarache on sun 6 aug 00
Hello all,
I am looking for the analysis of frit GF 106.
Could someone help.
Later,
Edouard Bastarache
Dans / In "La Belle Province"
edouardb@sorel-tracy.qc.ca
http://www.sorel-tracy.qc.ca/~edouardb/
Sharon31 on sun 6 aug 00
FRIT GF-106
Melts At: 1920F
Raw Weight: 344.23
ANALYSIS & UNITY FORMULA
CaO....... 0.33% [ 0.02]
MgO....... 0.70% [ 0.06]
Na2O...... 16.57% [ 0.92]
Al2O3..... 5.93% 0.20
SiO2...... 76.47% 4.38
>From The Magic Of Fire,\ Hansen, From another corner of Canada
From: Edouard Bastarache
To:
Sent: Sunday, August 06, 2000 05:16
Subject: Frit GF 106
> Hello all,
>
> I am looking for the analysis of frit GF 106.
> Could someone help.
>
> Later,
>
> Edouard Bastarache
> Dans / In "La Belle Province"
> edouardb@sorel-tracy.qc.ca
> http://www.sorel-tracy.qc.ca/~edouardb/
| |
|