Alisa and Claus Clausen on sun 6 aug 00
I made a mistake recommending my favorite clear glaze to Grace as an =
easy clear.=20
It was noticed thanks to a fellow clayarter Holly that pointed it out to =
me,
Ron Roy's satin matt=20
30 G-200
20 Walloastonite
30 EPK
20 3134
NOT 30 3134 as I originally posted,
Sorry, but try it now!
best regards,
Alisa in Denmark
Good luck