Alisa and Claus Clausen on mon 7 aug 00
Dear Clayart,=20
I would like to clarify that I am aware that some of the newly tested =
glazes I posted are intended for glaze 6 reduction.
The majority of them were posted my Marcia Selsor. =20
It is my purpose to see what they do in oxidation.
Because I had such good results with Hal's Pale Apple cone 7-10 =
reduction in cone 6 oxidation, I found Marcia's list a cornucopia of =
temptation. Often as it is, receipes designated for cone this, =
atmosphere that, can be flexible, with varying results, but results that =
may be of use. I am not recommending trying to see what happens to an =
04 glaze or eathernware body at cone 9! unless you need to redecorate =
with new kiln furniture.
These receipes are knowingly tested in oxidation to see what happens!
Marcia told me that there are people using them with great success in =
oxidation and I want to see first hand what can be acheived.
If someone wants to post their results of the same receipes in Redux. it =
would be interesting to compare results.
Best regards,
Alisa in Denmark.
| |
|