David Cowdrill on mon 7 aug 00
Michele: From the Operating Manual Err1 is: "Ramping up and rate is less
than 12 deg. per hour." Possible cause: " Kiln-sitter has tripped. Limit
timer has expired. Elements are weak. Load is heavy. Relay failed. Low
voltage."
When this happened on mine it was due to worn-out elements. After
replacing elements and thermocouple the kiln has worked normally.