Susan Wallace on fri 11 aug 00
Formula for Reeves Green, Cone 10:
Potash Feldspar.........75.0
Whiting.................15.0
Silica...................5.0
Kaolin...................5.0
100.0
Add: Chrome Oxide Green..4.0
Bentonite................2.0
My notes don't tell me if this glaze is for reduction or oxidation or both.