ASHPOTS@AOL.COM on wed 16 aug 00
Howdy all, well i fired again and the Axner Probe worked today. I did blow
into the ports for the wires.I guess that worked, thankyou.
It is hard for me in this old Alpine to get .55. I will open Thurs after the
110 mile yard sale.It starts at Gadsden Ala.
I was in a cave the other day and i found some red clay near it and i glazed
a pot using 50/50 clay and ash, i hope it works.
I need to start wearing gloves again with this ash glaze, my hands are
pealing.YIKES.
Capt Mark
PS Amy, I have to be a Capt this weekend. Do you and the girls want to go
for a Duck Ride???????????????
| |
|