play with the titanium dioxide

updated fri 25 aug 00

 

Sharon31 on thu 24 aug 00


Hi!
This glaze, I posted from Lana Wilson's book,
Crystal ^6/2 of Jeany Ritcher
==========================
FRIT 3110........................ 49
ZINC OXIDE ....................26
ENGLISH KAOLIN(Puraf 1.4
QUARTZ ..........................17.1
TITANIUM DIOXIDE....... 5.7
Has a variation
TITANIUM DIOXIDE ..........7
These days, I try, for the next crystalline firing, different colors, and
some changing in the base, decreasing the 3110 into another frit and
changing some materials.
Can you please tell me how much I can play with the TITANIUM DIOXIDE and
what will it make to the crystals?