Ann Brink on thu 24 aug 00


I've made similiar discs of stoneware, but for another reason...to place
under pots to prevent them sticking to shelves with old glaze drip spots on
them.

Ann Brink in Ca

----- Original Message -----
From: mel jacobson
To:
Sent: Thursday, August 24, 2000 4:43 AM
Subject: unknown clay


> the best way i have found is to fire the pot
> on a bisqued plate or catcher. susan karrisch
> fires many of her test pieces at the farm on
> a flat porcelain disc about an 1/8 inch thick.
>
> she just rolls them out, cookie cutter cuts them
> and has about 40 of them in her boxes.
>
> of course this is one of america's fine crafts persons.
> (butterflies, cm last december)
> mel
>
>
> FROM MINNETONKA, MINNESOTA, USA
> http://www.pclink.com/melpots (website)
>
>
____________________________________________________________________________
__
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.
>