search  current discussion  categories  glazes - misc 

4,3,2,1, glaze,

updated sun 27 aug 00

 

Wade Blocker on sat 26 aug 00


James,
A base glaze is usually a simple glaze to mix, with a few standard
ingredients. You can also substitute different colorants for those
given,eg. cobalt for the iron, or copper oxide. Use titanium oxide instead
of rutile, and see what happens. Mia in ABQ