search  current discussion  categories  kilns & firing - misc 

fwd: re: kiln question

updated thu 31 aug 00

 

mel jacobson on wed 30 aug 00


>From: Jim Larkin
>X-Mail-Agent: WebSage II, build 4930d
>Date: Wed, 30 Aug 2000 13:04:23 -0600 Central Daylight Time
>To:
>Subject: RE: kiln question
>X-MIME-Autoconverted: from quoted-printable to 8bit by mx1.mx.voyager.net
>id e7UI6Vp07337
>
>Lisa,
>I have a Bailey the same size as yours and get good results with the
>following firing schedule:
>(1) Pilot overnight with peeps in and damper 3/4 closed. By morning the
>temp. is approx. 500 degrees F.
>
>(2) In the morning, open damper fully, light both burners at 2 w.c.",
>blowers on full, and burner flaps closed or nearly closed, until the
>burners make a slight "bacon frying" sound.
>
>(3) At 800 degrees I adjust burners to 4 w.c." That is usually 30 min. to
>1 hour wait.
>
>(4) At 1000 degrees or so I adjust burners to 7 w.c.". That is usually 30
>min to 1 hour wait.
>
>(5) For copper reds I begin reduction at cone 01, for most glazes at 06.
>I create reduction by closing the damper about 3/4ths. Determination of
>final damper setting is made by watching the flame out the bottom peephole:
>I want a lazy but persistent licking flame there. You should also see
>intermittent licking flame past the damper. I leave this setting
>(sometimes having to make minor adjustments to the damper by watching the
>bottom peep flame) until cone 10 falls. For me this is usually about a 12
>hour firing, which is rather long for a kiln this small, but the results
>are good.
>
>For consistent copper reds it helps to relight the kiln at dull red and
>reduce heavily again for about 20 minutes.
>
>It is always a good idea to check your burner orifices to see if little
>insect critters have been at work plugging them up.
>
>Also, call Bailey and get advice from them. Good luck.
>
>Jim Larkin
>Fox Pass Pottery
>Hot Springs, Arkansas
>71901
>501-623-9906
>foxpass@aristotle.net
>
>----- Original Message -----
>-- From: mel jacobson
>-- To: CLAYART@LSV.CERAMICS.ORG
>-- Subject: kiln question
>-- Date: Wed, 30 Aug 2000 12:39:12 -0500
>
>
>Date: Wed, 30 Aug 2000 09:36:57 -0700 (PDT)
>From: lisa young
>Subject: re:baileykiln
>To: mel jacobson
>:
>:
>:
>
>
> I have a bailey 18/12 studio kiln which is very
>consistent but difficult to get past cone 9 and half,
>and difficult to get more than a trace of copper red.I
>have tried many different firing schedules, with no
>real change in result. The fuel is natural gas. Anyone
>got any ideas?
> thanks. Lisa Young
>--- mel jacobson wg.
> >
> >
> > clayart mail
> > melpots2@pclink.com
>
>
>__________________________________________________
>Do You Yahoo!?
>Yahoo! Mail - Free email you can access from anywhere!
>http://mail.yahoo.com/
>
>
>FROM MINNETONKA, MINNESOTA, USA
>http://www.pclink.com/melpots (website)
>
>______________________________________________________________________________
>Send postings to clayart@lsv.ceramics.org
>
>You may look at the archives for the list or change your subscription
>settings from http://www.ceramics.org/clayart/
>
>Moderator of the list is Mel Jacobson who may be reached at
>melpots@pclink.com.
>
>
>



FROM MINNETONKA, MINNESOTA, USA