: re: glaze of week for aug 31 2000

updated mon 4 sep 00

 

iandol on sat 2 sep 00


The comments of Ron Roy suggest that the notes given with this glaze =
need revision. If it is deficient in both Silica and Alumina it could =
hardly be called < The quintessential balanced glaze type > and is =
possibly better consigned to history. Having Gerstly Borate as an =
ingredient makes it obsolete anyway.