search  current discussion  categories  forms - handles 

exploding handles-help

updated mon 4 sep 00

 

Earl Brunner on sat 2 sep 00


This sounds more like the culprit to me. At the art center
I fire a schedule similar to yours, only I hold it at 190
just to be safer.

Louis Katz wrote:
>
> Hi,
> Two suspicions.
> One is that your kiln may say it is at 200 degrees but is actually above that
> temperature and the handles are blowing then.
>
>
--
Earl Brunner
http://coyote.accessnv.com/bruec
mailto:bruec@anv.net