dean warsing on fri 8 sep 00
does anyone use miller master glazes? does anyone know where it is sold?
thanks dean
Jennifer Assinck on fri 8 sep 00
Dean:
I have some Miller Masterglazes and their colour chart. The colour chart gives the
address as 8934 N. Seneca St., Weedsport, N.Y. 13166. However, I just checked
www.411.com and they are no longer listed in that state. They probably have gone
out of business.
Jennifer Assinck
Newmarket, Ontario
dean warsing wrote:
> does anyone use miller master glazes? does anyone know where it is sold?
> thanks dean
>
> ______________________________________________________________________________
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at melpots@pclink.com.
Scsclay@AOL.COM on fri 8 sep 00
<< does anyone use miller master glazes? does anyone know where it is sold? >>
Miller is owned by Laguna Clay. At least the clays are still around,
distributed
by them. I'm not sure about the glazes. Check their catalog or website.
| |
|