Alisa and Claus Clausen on sat 23 sep 00
Dear Diane,
Have you try to opacify a simple clear gloss with zircopax? 15%? tin =
for a less "hard" white.
Could be for you.
Otherwise, my whites are not for you, they are semi matts or have =
crystals.
So, for this maybe useless suggestion, do I qualify for the soup cracker =
category?!
Good luck,=20
Best regards,
Alisa in Denmark
| |
|