search  current discussion  categories  glazes - cone 4-7 

white glaze for ^6

updated wed 27 sep 00

 

Diane Mead on fri 22 sep 00


Hi everyone:

Would anyone feel like telling me their favorite, most streamlined
cone 6 white glaze, glossy. Pick one you know does a good job on
stoneware.

I will send cookies to the supplier of the best one (we will test what we
can).

Thanks, folks

diane mead
mt. de sales academy
macon, georgia
_________________________________________________________________________
Get Your Private, Free E-mail from MSN Hotmail at http://www.hotmail.com.

Share information about yourself, create your own public profile at
http://profiles.msn.com.

MOLINA, RAFAEL on tue 26 sep 00


The following recipe works well for me in ^ 6 oxidation:

Antique White ^ 6 oxidation from Peggy Heer

Volcanic Ash 35.0
Gerstley Borate 12.5
Kaolin 2.5
Ultrox 11.0
Whiting 12.0
Bentonite 0.5

Good luck! ;-D

Rafael Enrique


Rafael Molina, MFA
Assistant Professor of Art
Music, Art, and Dance Department
Tarrant County College-Southeast Campus
2100 Southeast Parkway
Arlington, Texas 76018-3144
(817) 515-3711
(817) 515-3189 fax