Don Pipes & Mary Van Peursem on fri 22 sep 00


Glazes for Liz whose address I have misplaced(along with my brain). =
They come from the Lansing Potters Guild(Michigan)
and are at least 25 years old. All are batch glaze portions(duh!)

Woo Ash
Potash spar 3000
Kaolin 900
Whiting 1500
Talc 240
Flint 740
Mixed wood ash 1500
Bone ash 240

RIO 243.6
*runs



Woo Tan Matt
Soda Spar 370
Dolomite 370
Whiting 50=20
Kaolin 370
Flint 80

*better in hotter part of kiln




Woo Segar
Feldspar* 1050
Flint 675
Ball 325
Whiting 450

4% RIO
4% Titanium dioxide

*This is one of those glazes where one dip gives one color and two =
another.
One spar gives rust/black, the other gives rust/blue.
Four glazes in one here!
Sorry, can't recall which is which but it is certainly worth testing.

That's a lot of typing!!
Regards
Mary Helen Van Peursem
Island Pottery
Padre Island
Corpus Christi, Tx 78418

Liz Willoughby on sat 23 sep 00


Thanks very much Mary. Better to post them on clayart anyway, so
others can try them out. That is a lot of typing.

Liz


>Glazes for Liz whose address I have misplaced(along with my brain).
>They come from the Lansing Potters Guild(Michigan)
>and are at least 25 years old. All are batch glaze portions(duh!)
>
>Woo Ash
>Potash spar 3000
>Kaolin 900
>Whiting 1500
>Talc 240
>Flint 740
>Mixed wood ash 1500
>Bone ash 240
>
>RIO 243.6
>*runs
>
>
>
>Woo Tan Matt
>Soda Spar 370
>Dolomite 370
>Whiting 50
>Kaolin 370
>Flint 80
>
>*better in hotter part of kiln
>
>
>
>
>Woo Segar
>Feldspar* 1050
>Flint 675
>Ball 325
>Whiting 450
>
>4% RIO
>4% Titanium dioxide
>
>*This is one of those glazes where one dip gives one color and two another.
>One spar gives rust/black, the other gives rust/blue.
>Four glazes in one here!
>Sorry, can't recall which is which but it is certainly worth testing.
>
>That's a lot of typing!!
>Regards
>Mary Helen Van Peursem
>Island Pottery
>Padre Island
>Corpus Christi, Tx 78418