search  current discussion  categories  glazes - misc 

dark clay, glaze

updated tue 26 sep 00

 

Karen Sullivan on mon 25 sep 00


byron temple white ^10

custer spar 1750
dolomite 938
whiting 125
kaolin 1150
flint 938

Glaze has a soft satin surface.

Otherwise on dark clays I love shino, pretty much any shino.
If someone were to ask me to define beauty, my response would be shino.
The meaning of life? shino
The path to happiness? shino
Fill in the blank...you got it...shino

bamboo karen

I am still mystified about the computer crashing yesterday, with the screen
saying "Ceramics suck" then a horrible winding down sound as everything went
blank.
I do not understand the sensibility of those who inflict discomfort and
harm.

take care...