crater glaze

updated fri 6 oct 00

 

will edwards on wed 4 oct 00


I am not positive where I got this from but it supposed to be a ^6 crater=

glaze. I do remember someone telling me it came from a CM article. Should=
you
have luck with it, let us all know.

W. Edwards

Cryolite--33% =

Zircopax--67% =


Add Bentonite--2% =