spray foam packaging

updated sun 8 oct 00

 

Pierre Brayford on sat 7 oct 00


This product is used here in the UK by builders (and me) to secure wooden
window frames in the opening in the brickwork.

To make sure that it sets reasonably quickly the area is first sprayed with
water - moisture seems to be important to the curing process