Ron Roy on thu 19 oct 00
Looks like G200 is the closest - both have more SiO2 than Norfloat. Mail me
the recipe off list and I can convert to either. If you have a calculator I
can send my analysis of Norfloat and you can do your own.
Something I have been meaning to ask for a while now - would anyone sending
me Email on or off list - please put my Initials (RR) in the subject line.
I am deleting as fast as I can these days and I'm sure I am missing some
personal messages - I just can't read em all.
RR
>Hi. A student is about to mix up a glaze from an old book Recipe not
>available tonight..) It calls for norflot spar. What is the proper sub? I
>suggester Custer or G-200. Any info out there?
>Hanks in advance (TIA) Bonita in San Francisco
>www.cpmg.com/anagama
>
>______________________________________________________________________________
>Send postings to clayart@lsv.ceramics.org
>
>You may look at the archives for the list or change your subscription
>settings from http://www.ceramics.org/clayart/
>
>Moderator of the list is Mel Jacobson who may be reached at melpots@pclink.com.
Ron Roy
93 Pegasus Trail
Scarborough
Ontario, Canada
M1G 3N8
Evenings 416-439-2621
Fax 416-438-7849
| |
|