Jonathan Kaplan on wed 25 oct 00


Looking for a translucent porcelain/china/bone china casting recipe for
cone 6 or cone 10.

I'll be glad to reciprocate if I can provide any information.

Best


Jonathan

Jonathan Kaplan
Ceramic Design GroupLTD/Production Services
PO Box 775112
Steamboat Springs, CO 80477
(970) 879-9139 voice and fax
http://www.sni.net/ceramicdesign

UPS: 1280 13th St. Unit13
Steamboat Springs, CO 80487

Francoise Bazard on fri 27 oct 00


Hello Jonathan,
I can give you two formulas for porcelaine (cone 10) you can find in
Daniel Rhodes book :
Feldspar 85
whiting 15
= 100

and :
feldspar 60
silica 20
whiting 20
= 100

I hope it will help you
Best regards
Francoise
--