Arnold Howard on wed 1 nov 00


Paragon will soon introduce a front-loading, cone 10 kiln for potters. I saw
the first prototype yesterday and was impressed with the heavily-insulated
walls. We are pricing the kiln for tight budgets.

For more information, please send me an email.

With best wishes,

Arnold Howard
Paragon

__________________________________________________
Do You Yahoo!?
>From homework help to love advice, Yahoo! Experts has your answer.
http://experts.yahoo.com/

Veena Raghavan on fri 3 nov 00


Hi Arnold,
I saw your post about the new front loading Cone 10 kiln. As you
may recall, I am one of the "short potters" who replied to your original
query and would definitely be very interested. So, may I please have more
information.
Thanks in advance.
Veena

Candise Flippin on thu 9 nov 00


Hi all!

I received this yesterday from Paragon and it looks very interesting. This
kiln design has elements on three walls and I am curious about how this
might effect even heating.

Thanks, Candise in San Diego

-----Original Message-----
>I am listing the specs below...

>Please let me know what you think of the kiln.


24" wide x 24" deep x 27" tall,
9 cubic foot interior
4" walls and top, 4 ½" bottom
Mercury relays
Digital controller
1/4" diameter type K thermocouple
Two tapered peepholes in side,
1” vent hole in top
28" tall, heavy duty stand included
240 & 208 volt, 1 & 3 phase
240 volt, 1 phase model:
69 amps, 16,500 watts;
80 amp circuit breaker required
Shipping weight:
kiln - 825 lb. Stand - 150
Suggested retail $3,900