search  current discussion  categories  glazes - cone 8-10 

cone 10 ox glaze test url's

updated fri 3 nov 00

 

Wesley C. Rolley on thu 2 nov 00


I was a little quick on the mouse finger and sent the test descriptions
before I plugged in all of the URL's.

For the Deerpark glaze:

http:www.refpub.com/assets/glaze/dpin.jpg - shows pooling and frosty area
on the inside.
http://www.refpub.com/assets/glaze/dpout.jpg - outside of the same sakezuke.

For the Shahn glaze:

http://www.refpub.com/assets/glaze/shahn.jpg.

Shows the flow of the glaze. Pinched/scraped yunoumi with some faceting
that is shown off by the glaze. I should have slipped this one.

For the Harpersfield glaze:

http://www.refpub.com/assets/glaze/harpers.jpg

Wes Rolley
Wes Rolley

"Happiness is to be fully engaged in the activity that you believe in and,
if you are very good at it, well that's a bonus." -- Henry Moore

http://www.refpub.com