search  current discussion  categories  materials - frits 

sodium frit for cadycal sub

updated fri 10 nov 00

 

Craig Martell on sat 4 nov 00


Hi:

Donald asked about sources of sodium when subbing Cadycal for Gerstley
Borate. I think that Fusion Frit # F-435 would be a good one to use. It's
a high sodium frit with no boron.

regards, Craig Martell in Oregon

Mark/El Rossier on wed 8 nov 00


Francis,

I use Ferro 3110 and so far in tests it works fine.

----- Original Message -----
From: Craig Martell
To:
Sent: Sunday, November 05, 2000 12:26 AM
Subject: sodium frit for Cadycal sub


> Hi:
>
> Donald asked about sources of sodium when subbing Cadycal for Gerstley
> Borate. I think that Fusion Frit # F-435 would be a good one to use.
It's
> a high sodium frit with no boron.
>
> regards, Craig Martell in Oregon
>
>
____________________________________________________________________________
__
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at
> melpots@pclink.com.
>