search  current discussion  categories  materials - barium 

strontium, ken

updated sat 11 nov 00

 

Alisa and Claus Clausen on fri 10 nov 00


Dear Ken,
I do not have any Strontium now, as it is not something my supplier =
keeps on the shelf. That is why I always sub. with Barium Carb.
But,. my supplier just imformed that he can get it, but I do not know =
from where. Must be our only importer, Cerama. If this is true,
I will send you their address, or rather here it is and you contact them =
cerama@cerama.dk and www.cerama.dk . They of course speak
English, (I think!). If you need help, write to me at =
alisajo@privat.dk.
Best regards,
Alisa in Denmark

Ababi Sharon on fri 10 nov 00


My supplier, just lately started to import it .Before, I ordered it from the
U.S.A.. You use it to foodsafe glaze. For decoration, use Barium carbonate,
1.33 of the strontium, Just don't smoke or drink when you work with
it.(better not smoke at all)
ababi
----- Original Message -----
From: "Alisa and Claus Clausen"
To:
Sent: Friday, November 10, 2000 9:56 PM
Subject: Strontium, Ken


Dear Ken,
I do not have any Strontium now, as it is not something my supplier keeps on
the shelf. That is why I always sub. with Barium Carb.
But,. my supplier just imformed that he can get it, but I do not know from
where. Must be our only importer, Cerama. If this is true,
I will send you their address, or rather here it is and you contact them
cerama@cerama.dk and www.cerama.dk . They of course speak
English, (I think!). If you need help, write to me at alisajo@privat.dk.
Best regards,
Alisa in Denmark

____________________________________________________________________________
__
Send postings to clayart@lsv.ceramics.org

You may look at the archives for the list or change your subscription
settings from http://www.ceramics.org/clayart/

Moderator of the list is Mel Jacobson who may be reached at
melpots@pclink.com.