Our plant has concrete floors and we first use a push broom with lots of
sweeping compound to do a first clean up. Then we use our Nilfisk GS 80
vacuum to take care of the rest. Finally, we wet mop the entire floor any
number of times and the results are quite nice, at least for a while!