search  current discussion  categories  glazes - cone 8-10 

glaze request: cone 10 humboldt orange, breaks blue

updated tue 14 nov 00

 

Sabra Wood on sun 12 nov 00


> if anyone has heard of this claze, or has a similar recipe, please let me know.
> thanks

June Perry on mon 13 nov 00


Look in the archvies for Woo Blue/Brown, or any other chun type base that has
rutile and iron as the colorant.
Moonlite, also in the archives on an iron bearing body will give your the
blue/orange you're looking for. Both are cone 10 glazes.

Regards,