search  current discussion  categories  glazes - specific colors 

sv: emerald green

updated sat 18 nov 00

 

Alisa and Claus Clausen on fri 17 nov 00


Hi,
Using the additive colorants from the above glaze,
=20
2 chrome oxide=20
1 cob. carb.

I have tested both "store bought" and mixed in the lab clears, and the =
resulting color has been very similar.

If you need some bases, post me off line
alisajo@privat.dk

Best regards,
Alisa