If it has no iron and is not reduced it is not a celadon glaze.
It may be a celadon like glaze or a celadon colored glaze.
What we call a celadon is a glaze that the Chinese invented it and it
had some iron in it, not cobalt, not copper and not Mason stain.

Rant off.

Rick Mahaffey

Diane G. Echlin on tue 21 nov 00


Thanks, Rick! I've been following this thread hoping someone would
clarify for me what constitutes a celedon! One more question, though:
does the firing atmosphere and/or temp influence whether it is truly a
celedon?
Diane in CT

rickmahaffey wrote:
>
> Folks,
>
> If it has no iron and is not reduced it is not a celadon glaze.
> It may be a celadon like glaze or a celadon colored glaze.
> What we call a celadon is a glaze that the Chinese invented it and it
> had some iron in it, not cobalt, not copper and not Mason stain.
>
> Rant off.
>
> Rick Mahaffey
>
> ______________________________________________________________________________
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at melpots@pclink.com.