Good Grey Celedon, George Lowe, Cone 10

custer spar 25.3
kona F-4 11.5
flint 28
whiting 6.4
kaolin 5.2
gerstley 5.8
borate
barium carb. 6.3
dolomite 5.8
zinc 1.3
zircopax 3.7
iron ox. 0.5
cobalt carb. 0.007

bamboo karen