Alisa and Claus Clausen on mon 27 nov 00
Source Clayart (Brian Gartside, N.Z.)
=20
Tested on white mid range stoneware, fired to 1220c, oxidation. =20
=20
Receipe
4 parts Borax Frit
4 parts Clay
2 parts Silica
2 parts Feldspar potash
1 part Whiting
1 part Talc
Substitutions
Ball clay for clay(?)
Local spar for potash
=20
Resulted in stable, clear to white high gloss.
=20
Personal: This was making cookies, Mel. I really sort of dug in the =
sack and dumped and mixed and it worked. =20
=20
Best regards,
Alisa in Denmark
| |
|