glaze test for willliam edwards cone 6 clear, oxidation, cone 6.

updated tue 28 nov 00

 

Alisa and Claus Clausen on sun 26 nov 00


Source: William Edwards.
Tested on white, mide range stoneware, fired to 1220c, oxidation. =20

Receipe:

12.50 Whiting
12.50 EPK
20 Neph. Sye.
25 Frit 3134
30 Flint

Substitution
Local frit for 3134

Results
Stable, glossy clear. No discernable difference where dipped twice.