search  current discussion  categories  kilns & firing - coatings 

itc - electric kilns?

updated fri 8 dec 00

 

Susan Hubele on thu 7 dec 00


ITC sounds like a wonderful product in terms of
increasing a kiln's efficiency. I have, however,
heard reports of ITC fusing the elements to the
softbrick of an electric kiln, making it
impossible to remove the elements for
replacement/repair.

I suspect this must be related to the application
method. Can anyone please comment on their
experience with this?

Thanks.

Susan
___________________________________________________
Susan Hubele
Box 906
Cochrane, Alberta
Canada T4C 1A9

T: (403) 932.2470
F: (403) 932.9233
E: shubele@foff.com

View Susan's ceramic art: http://www.foff.com
____________________________________________________