search  current discussion  categories  glazes - specific colors 

sv: adelaide robineau's elusive black slip

updated fri 8 dec 00

 

Alisa and Claus Clausen on thu 7 dec 00


Dear Beth,
Shot in the twighlight..The best collection of her work I have seen is =
at the Everson Museum in Syracuse New York,
They may have that sort of information or give you some other leads. =
Let us know, it would be interesting to hear.
Best regards,
Alisa in Denmark

>
> I am currently on the hunt for Adelaide Robineau's black slip =
recipe
>which she often used over her carved porcelain pieces. Anyone have any
>leads?
>
>
> Beth Cavener Stichter
>
>________________________________________________________________________=
______
>Send postings to clayart@lsv.ceramics.org
>
>You may look at the archives for the list or change your subscription
>settings from http://www.ceramics.org/clayart/
>
>Moderator of the list is Mel Jacobson who may be reached at =
melpots@pclink.com.
>