michael wendt on thu 7 dec 00
Hi Clayarters
If you don't use grog, or calcined Kaolin, or hate surveys, delete this =
message now.
I have had an inquiry that has me thinking about adding a continuous =
calciner to our operation here in Lewiston, Idaho to produce Helmer grog =
and calcined Helmer Kaolin. If you want to participate in this use =
survey,email me or print out the message below and fax it to me at our =
toll free fax number or mail it to the address below. Your response will =
help me to work out the size of calciner needed to meet demand. Too =
small and there will be order delays, too large and the cost of the =
equipment will be too high to be covered by sales.
email to: wendtpot@lewiston.com
Fax to: Michael Wendt, Wendt Pottery/ Idaho Clay and Glaze =
1-888-554-3724 or mail to:Michael Wendt, Wendt Pottery/ Idaho Clay and =
Glaze=20
2729 Clearwater Avenue , Lewiston , Idaho 83501
1. How much grog do you use per year?______________
2. How hot do you want it fired?____________
3. How much calcined Kaolin do you use each year?______________
4. How hot do you want it fired?_____________
5. Would the presence of some colloidal iron pose a problem?__________
6. What mesh sizes of grog do you use and in what quantities?
__________________________________________________________
7. What mesh sizes of Calcined Kaolin do you use? __________ =
Quantities______
8. Any other comments are appreciated.
Name_________________ Address___________________ City _______________
St.________ Zip___________
Thanks for your help,
Regards,
Michael Wendt wendtpot@lewiston.com
| |
|