search  current discussion  categories  glazes - cone 4-7 

glaze test for f. carlton ball rust orange, cone 5-6,

updated tue 12 dec 00

 

Jean Todd on tue 12 dec 00

oxidation.

Never had so many replies before. Thankyou everyone, but really, I
feel I should have been able to work this one out, must be one of
those senior moments.
> Jean,
>
> I expect you'll get tired of hearing this, as you'll get loads of
> replies , but RIO is red iron oxide. We need to be more careful
> of using so many abbreviations, don't we?
>
> Cindy Strnad
> Earthen Vessels Pottery
> RR 1, Box 51
> Custer, SD 57730
> USA
> earthenv@gwtc.net
> http://www.earthenvesselssd.com


Jean from Cowra, NSW
"Lang may your lum reek"
mallyree@ix.net.au