search  current discussion  categories  glazes - traditional iron glazes 

thick white shino

updated thu 14 dec 00

 

Donald G. Goldsobel on wed 13 dec 00


To Shino lovers and glaze formula collectors- can you help?


I had a recipe for a glaze tha was named Thick White Shino
and I have misplaced the formula. I have plenty of Shino recipes, but
this one in particular has the characteristics of a Nuka, but has a more
glassy surface at its edges and develops gteat gey to white tones.


Does anyone have this recipe?


TIA