Dear Will,
Wax the edges before they dry. This prevents them from drying much
faster than the center.
Marcia
who prefers sheet rock
will edwards wrote:
>
>snip
> Perhaps drywall is for some who are willing to do the flipping and the wire
> racks are for others who have figured out the best method for that.
> Its always good to hear both the pro's and con's of how to do things so we can
> narrow down the process of invention.
snip
They also claimed that the "drywall sandwich"
> process didn't work at all for them." <<>
> My thought is the edges seem to dry the quickest and regardless of how much
> air we have around them it never has given up the flatness we would desire.
> The weight of the board would not only slowly remove moisture from the pieces
> snip I bet they must turn the
> tiles every so often and it is quicker for them that way?
>
> William Edwards
> Opelika Arts Center
>
> ____________________________________________________________________
> Get free email and a permanent address at http://www.netaddress.com/?N=1
>
> ______________________________________________________________________________
> Send postings to clayart@lsv.ceramics.org
>
> You may look at the archives for the list or change your subscription
> settings from http://www.ceramics.org/clayart/
>
> Moderator of the list is Mel Jacobson who may be reached at melpots@pclink.com.
--
Marcia Selsor
selsor@imt.net
http://www.imt.net/~mjbmls
http://www.imt.net/~mjbmls/Tuscany2001.html
| |
|