here's the formula for bbv clay

updated tue 19 dec 00

 

June Perry on mon 18 dec 00


71.3 SiO2
1.5 TiO2
18.8 Al2O3
0.08 Fe2O3
0.3 MgO
0.2 CaO
0.3 Na2O
1.9 K2O
Loss 4.9